Mechanical properties of cold-rolled non-grain oriented electrical steel of conventional quality in accordance with GOST 21427.2-83
| Steel grade |
Density, kg/dm3 |
Guaranteed properties |
Typical properties |
| HV5 |
Tensile strength σB, N/mm2 |
Elongation, δ4, % |
Number of Bends, |
Lamination factor, % |
HV5 |
Yield point σT N/mm2 |
Tensile strength σB N/mm2 |
Elongation, % |
Number of bends |
Lamination factor, % |
| 2411-2414 |
7,60 |
140-210 |
370-600 |
15-30 |
2 |
0,96 |
190 |
368 |
494 |
20 |
>5 |
0,97 |
| 2312 |
7,70 |
120-160 |
330-470 |
20-35 |
3 |
0,96 |
168 |
323 |
476 |
27 |
>5 |
0,97 |
| 2216-2211 |
7,75 |
120-145 |
300-450 |
20-35 |
3 |
0,96 |
127 |
221 |
391 |
31 |
>10 |
0,97 |
| 2111-2112 |
7,80 |
110-145 |
300-450 |
20-35 |
- |
0,96 |
124 |
234 |
394 |
30 |
>10 |
0,97 |
| 2011-2013 |
7,82 |
120-160 |
290-490 |
15-35 |
- |
0,96 |
123 |
243 |
404 |
30 |
>10 |
0,97 |
|
|
|